Monday, June 27, 2016

Re: [MW:25015] COMBINATION PROCESS WPS

Dear Sir

As per your mentioned to make a new WPS & PQR to support GTAW for our reference, do they any code for reference? Please advise

Best Regards


Suchin K
+66 81 889 4912

Sent from my iPhone

On 26 มิ.ย. 2559, at 21:02, Hareesh K V <hareesh13h@gmail.com> wrote:

Dear sir,

You have to make a new WPS (say WPS-B) with the same PQR.

The issue in using the same WPS is, we cannot identify whether the joint is welded with full GTAW or with GTAW+SMAW.

Regards,
Hareesh K V
+91-8547859202


Sent from my Samsung Galaxy smartphone.
-------- Original message --------
From: "Vanchinath S.A." <vanchinaths@gmail.com>
Date: 26/06/2016 2:10 pm (GMT+05:30)
Subject: Re: [MW:25005] COMBINATION PROCESS WPS

Revise WPS with existing PQR.

On 26 Jun 2016 2:07 p.m., "balaji srinivasan" <bolukbalaji@gmail.com> wrote:

Dear all,

We have WPS-A for stainless P8 to 08  witith Gtaw+ smaw thickness limit is gtaw 8mm and smaw 14mm.
Now our construction team is trying to weld only gtaw process for upto 8mm weld joints with same WPS -A .
Is it possible to use it or I want make new WPS for gtaw with supporting of same PQR.
Please advice.

Regards,
Balaji.M

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAK1csg3c12yx1TKv2e017UVobthBT5YWAkD9UMGjC2ricpWbHA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2B6Tn1Lp92GHE1ok3kKyLOuvLqdAGEuzTE386BD-qUKV%3DQqtpA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/453q5uajcnluq1au7k3yg804.1466949686833%40email.android.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...