Re: [MW:24984] Probe selection for UT flaw detection on steel casting

What kind of casting? Steel casting? What kind of material? What is the grain size? You may have a look in SA-609. You will find this spec in ASME BPVC Section II-Part A (second volume)

2016-06-19 9:40 GMT+03:00 manivannan hemu <hemumanivannan@gmail.com>:
Dear Experts
,
Please clarify me the following:

1. How to select right frequency, size of probe  to be selected for UT flaw detection particularly for steel castings?
2. Is it correct to use dual crystal probes for higher thickness [greater 100 mm] ? Is there any selection criteria on single crystal or dual on the basis of thickness, and its  limits recommended - Please provide your answer with supporting reference.

Thanks,
MANIVANNAN.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9bb8c8dd-7c96-4ff3-b5ef-bcdb5c6d7030%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40CJyHeG3i2iKmaBrKb0hfNTJ1f7XNyk8u1a6ptmS%2BbK3g%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...