Codes are not handbooks. Metallurgy knowledge is necessary.
In general CS needs to be buttered with an alloy which is not sensitive to sensitization from one part and from the other part does not give low FW. Then PWHT is performed and then SS us welded

Sent from my BlackBerry 10 smartphone.
From: Kumar Sajesh
Sent: Κυριακή, 29 Μαΐου 2016 - 16:02
To: materials-welding@googlegroups.com
Reply To: materials-welding@googlegroups.com
Subject: [MW:24903] PWHT req in dissimilar material welding


hi,

in a dissimilar welding between CS and SS, and if CS have PWHT requirement, what shall we do.
any code referances?

--
Regards,

Sajesh Kumar S

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMcH%2Bbb3_wxFNEiM3w6pp0WgLsFL8qYCz5eadHhzZHGLnWneUg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...