Re: [MW:24913] RE: 24908] IS 2062 safe working temperature

dear experts

thank you very much..

On Tue, May 31, 2016 at 9:12 AM, MW <raghurambathula@gmail.com> wrote:
up to 343 °C for ASME Sec VIII div1 vessels (not permitted for Section I and III)


On Tuesday, 31 May 2016 07:35:09 UTC+4, Kadir godil wrote:
its a vessel, max temperature will be 160 deg. C and pressure will be 5 Bar..

is there any standard or reference document which mentions its safe working temperature?



On Mon, May 30, 2016 at 6:13 PM, Lakshman Kumar. B <lakshmankumar4@gmail.com> wrote:

For which application and in which form?

 

Thanks & Regards,

Lakshman Kumar B,

+91 9440031459.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Kadir godil
Sent: Monday, May 30, 2016 5:29 PM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:24908] IS 2062 safe working temperature

 

dear experts,

 

what is the safe working range of IS 2062 steel? 

 

please inform me about the standard where i can find this data?

 

thank you

 

sincerely,

kadir godil



--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4b0484ab-db07-4fec-a4e4-18ec9db5a770%40googlegroups.com.

For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKaLp%2BXwqeMXb%2BKEEQuNrOA%2B1Tq%2BLnit9kru%3DXHYJdLYxLvGBA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...