Monday, May 30, 2016

Re: [MW:24910] RE: 24908] IS 2062 safe working temperature

its a vessel, max temperature will be 160 deg. C and pressure will be 5 Bar..

is there any standard or reference document which mentions its safe working temperature?



On Mon, May 30, 2016 at 6:13 PM, Lakshman Kumar. B <lakshmankumar4@gmail.com> wrote:

For which application and in which form?

 

Thanks & Regards,

Lakshman Kumar B,

+91 9440031459.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Kadir godil
Sent: Monday, May 30, 2016 5:29 PM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:24908] IS 2062 safe working temperature

 

dear experts,

 

what is the safe working range of IS 2062 steel? 

 

please inform me about the standard where i can find this data?

 

thank you

 

sincerely,

kadir godil

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b6c8669d-2e39-4058-a120-42eeba9651d2%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/007301d1ba70%24da40d340%248ec279c0%24%40gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKaLp%2BW7uFO5uwWkxoGdTz1EwggYVFsSn%3DKqu-FSY%3D60OyfqVQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...