Dear all,


Thanks for your inputs.


This tank we are using for food storage (Extreme Hygienic).


Please tell me what are the issues if we weld SS904L with SS304? SS904L have low carbon while SS304 is having high carbon content.


Will there be any issue of iron contamination in future which may be non-hygienic for food applications?


On Saturday, 28 May 2016 08:25:22 UTC+5:30, George Dilintas wrote:
no problem with 308 in that case

2016-05-26 20:29 GMT+03:00 Mohd Siraj <mohd...@gmail.com>:
what filler to be used for joining?

is 308L is okey?

On Tuesday, May 24, 2016 at 8:50:43 PM UTC-7, Makrand Sakpal wrote:

Dears,


We have one atmospheric hygienic (Food Industry) vertical vessel of SS904L material which is supported on legs. Vessel diameter is 3200 mm & TL-TL is 5100 mm.


The question is, can we weld SS304 directly on SS904L so that we can use SA-312 TP304 pipe l;eg supports?


Is it necessary to have SS904L RF pad instead of SS304?


Can there be an issue with weldability of SS904L with SS304?


Note : - We can't go for skirt support option.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/409451da-9d6f-4f95-9637-76f23c2fa9eb%40googlegroups.com.

For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f50b94fd-d17d-407e-9b44-9dffe1d940ed%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...