Monday, May 23, 2016

Re: [MW:24837] Metallurgical affect / defect clarifications

Forming of non tempered martensite and formation of cracks

Sent from my BlackBerry 10 smartphone.
From: 'nawab ali bhatti' via Materials & Welding
Sent: Παρασκευή, 20 Μαΐου 2016 - 05:37
To: Materials-welding
Reply To: materials-welding@googlegroups.com
Cc: materials-welding@googlegroups.com
Subject: [MW:24813] Metallurgical affect / defect clarifications

Dear Experts



We have one project, Material is Alloy P22, A335 (Cr2.25 and Mo 1), Customer requirement 
where heat treatment of low alloy steel is required the weld joint shall be immediately heat treated without allowing it to cool below 150C (300F). if this is not practical the weld and adjacent pipe shall be uniformly heated to min 300C (570F), kept for 20 minutes , wrapped with insulation allowed to cool and heat treated later"

Please tell me what will be metallurgical affect in weld area if above condition will not follow, only maintain preheat temperature 200C during welding as per WPS/ PQR and conduct the PWHT after one or two days

Best Regards




--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/936617816.5150279.1463694788989.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...