Monday, May 23, 2016

Re: [MW:24837] Ferrite % 4-8 of E309LMo

The purpose of this filler metal is to avoid hot cracking. This is achieved by giving at least Ferrite no 5

Sent from my BlackBerry 10 smartphone.
From: SATISH SHAH
Sent: Σάββατο, 21 Μαΐου 2016 - 05:51
To: Materials & Welding
Reply To: materials-welding@googlegroups.com
Subject: [MW:24816] Ferrite % 4-8 of E309LMo

Dear Expert,

Let me know Ferrite 4 - 8 % is possible to obtain of Electrode 309LMo as weld condition.


Regards

SATISH SHAH

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8c7f5e73-c5e0-4c60-ab4f-92cb2537713b%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...