Depends on your clients specification.  If impact testing is to be performed in accordance with A/SA-370, Table 9 allows multiplication of acceptance criteria by ratio of tested specimen to full size specimen (0.40 in your case).  Further, B31.3, Table 323.3.5 note (2), also allows for applying a ratio to the acceptance criteria for subsize specimens.  In looking at the information provided, you have met the required temperature reduction requirement specified in Table 323.3.4. 

 

In my opinion, a reasonable client should accept the values as meeting their specification requirements.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Kannayeram Gnanapandithan
Sent: Monday, May 23, 2016 8:19 AM
To: materials-welding
Subject: Re: [MW:24831] Impact Test Acceptance Criteria for Dissimilar material PQR qualification

 

Gr 2 will have less value compare to Gr1

On 23-May-2016 6:42 pm, "'Biplab Pal' via Materials & Welding" <materials-welding@googlegroups.com> wrote:

Dear Gents,

 

Our Construction Code is ASME B 31.3.

 

Our Client standard is asking for the minimum impact value of 34/27 J for P1 Gr 1 & 40/32 J for P1 Gr 2 full size (10X10) specimens both Weld metal and HAZ at minimum design temperature for PQR qualification.

 

Process- GTAW + SMAW

 

Out MDMT is -45 Deg C.

 

The PQR tested at -64.7 deg C and the impact values are as follows for Weld 20.33/17 J and for HAZ-1 is 41.5/35.5 & HAZ-2 is 40/50 J.

Specimen size is 10X4.

 

Is the test result acceptable for Weld zone as per client std.?

 

We need your kind advice and code reference.

 

 

--

Thanks & Regards
Biplab Pal
Welding Inspector

E-mail:   biplab.mech@gmail.com
 
Information in this email and any attachments is confidential and intended solely for the use of the individual(s) to whom it is addressed or otherwise directed. Please note that any views or opinions presented in this email are solely those of the author and do not necessarily represent those of the Company. Finally, the recipient should check this email and any attachments for the presence of viruses. Myself accepts no liability for any damage caused by any virus transmitted by this email.
 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFnzQg16oapSEhmVg6PdCf2_xhTdhmD5Kc50ojctYshM3tS1cA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOBEEL_ymoFUonWf-kCmc0P1LpeKf0%3DvchzAjFnxd%3DAsA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...