As per ASME Section VIII Div1, 
Please refer to the para UCS-56 (Requirements for Postweld Heat Treatment) para f(4)-a
Mentioned as maximum bead width shall be four times the electrode core diamter.

Best Regards,
Chandra

On 21-May-2016, at 2:28 PM, haundpvcms2016@gmail.com wrote:

I am wondering if anyone knows what the maximum weave is for SMAW (specifically ASME Section VIII Div 1). For some reason 3x is sticking in my brain, but I would like to know where to find it in the ASME Codes. 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/24ee9b7d-4956-4f4d-8a40-86b41259ea8f%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...