[MW:24906] BOLT& NUTS CONCERNS

Dear All.

There are some issues and concerns about bolt and nuts:(please mentioned reference document)
1.If the ring gaskets are lubricated and bolt tightening have been done and no leaks observed during hydro testing, is it accepted or not?if not flanges must loose?

2.Unfortunately after tightening, C.S bolts and nuts are painted.is there a document that painting forbidden or not (especially for sour service)?

3.B7M bolt and nut have rusted before tightening, are they must be derusted or not& how?rusting can affect on torque value? and regard to any leakage observed can be assured that min required tension are applied on bolts?

4.Is there a technical document that investigate effectiveness of Hammer tightening vs. of wrench and tensioner?

Regards.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALcH7WDU%3DpPFJUSS7K5s7pqR1QoYo-nLVHpvqKiAMfH0BXEi1w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...