U can carry out PWHT as per table   UCS 56.1 - Decrease the temperature  & increase the soaking time.

From: Kumar Sajesh
Sent: ‎29-‎05-‎2016 06:32 PM
To: materials-welding@googlegroups.com
Subject: [MW:24903] PWHT req in dissimilar material welding


hi,

in a dissimilar welding between CS and SS, and if CS have PWHT requirement, what shall we do.
any code referances?

--
Regards,

Sajesh Kumar S

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMcH%2Bbb3_wxFNEiM3w6pp0WgLsFL8qYCz5eadHhzZHGLnWneUg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...