Hi All ;
As per the latest Edition of ASME B31.3 2014 all materials for PNo 1 are exempt from PWHT .I don't have a current copy but this is the link

http://www.eng-tips.com/viewthread.cfm?qid=381691



On Tuesday, 26 January 2010 17:33:23 UTC+8, Nandesh Kumar wrote:
Dear All,
 
For our LNG piping project, as per ASME SEC IX for a pipe 16 inch OD and Thk 21.44 mm PWHT is manadtory? We are welding root and hot pass TIG and others SMAW.
Material is ASTM A333 .
 
Thaks in advance
Nandesh Kumar A


Your Mail works best with the New Yahoo Optimized IE8. Get it NOW!.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7c53cbab-7caf-4c08-a2cc-2ddccafecc6a%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...