Dear Gentlemen,

My client requirement is SA266Gr.2 with alloy625 weld overlay (Tubesheet), actually i want to prepare WPS & PQR verified with ASME Sec IX but i am not clear still i have some doubts, regarding point no:
1. What is the appropriate filler/electrode for 1st layer and subsequent layer.
2. What is the basemetal & weld metal qualification range.
3. What are the things i have to follow during preparation of WPS & PQR.

 Your response is highly appreciated.

Regards,
Venkkatesh Gopalakrishnan

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/08361262-c03f-40a3-8cc9-5900e01bbe9d%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...