Thursday, December 31, 2015

Re: [MW:24018] DIFFERENCE BETWEEN EN-287 OR EN-9606.

Dear Uday

This British Standard is the UK implementation of EN ISO 9606-1:2013. It is identical to ISO 9606-1:2012. It supersedes BS EN 287-1:2011 which is withdrawn.


On Thursday, 31 December 2015 8:11 AM, udaya bhaskar <dusroni@gmail.com> wrote:


Dear sir,

As per EN Stander we need to do WQT.

kINDLY SUGGEST  WHICH STANDERS TO BE FOLLOW ON THESE TWO-EN-287 OR EN-9606.
kINDLY LET US KNOW THE DIFFERENCE BETWEEN THESE TWO


--
uday
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANii3ROLaM9-TLnWAkwj4cyFczMKjJGq8hf9M6aBOjY7Sq8MWA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...