Monday, December 21, 2015

RE: [MW:23989] UG84.6 IMPACT SPECIMEN CLARIFICATION

A few questions.

Is the GTAW pass your root pass?

If so is it consumed by hot pass?

What's your primary process after the GTAW?

Is your weld joint welded from one or both sides?

 

 

Jim Price | Welding Engineer, CWI

Direct:  320.7463439 | Fax: 417-862-5564

jimprice@polarcorp.com

 

 

 

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of venkat guru
Sent: Monday, December 21, 2015 9:40 AM
To: materials-welding@googlegroups.com
Subject: [MW:23987] UG84.6 IMPACT SPECIMEN CLARIFICATION

 

Hi sir,
This is venkatesan from singapore.

Could you please clarify on the requirements of ASME Section Viii Div.1 Edition 2013 Section UG84.6?

PQR Base material : SA516 Gr.70 of thickness 38.1mm
Deposited weld metal like GTAW-4mm+SMAW-15mm+SAW-19.1mm

Question: HAZ impact specimen suppose has to be taken based on UG84.6, definitely GTAW process is difficult to cover.

Do we have to take impact for each process or just follow UG84.6 table?

Simply means, Impact test specimen will take for PQR/ PTC as per ASME VIII. Is based on thickness or process?

Thanks
Venkatesan

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACoj_XRQdZdqQqrxNhqVX6cWt972jkX_DzarDxxFSkUtyG3Fqw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...