Re: [MW:23984] ASME B31.3_2014 Minimum thickness for PWHT

No welding should be carried out below 10 degree Celsius, u have welding is done at above 10 degree 

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY

On Sun, Dec 20, 2015 at 7:53 AM, sajid sakhidas <sajidsakhidas@gmail.com> wrote:


Hi...;
we refer to ASME B 31.3 latest issued (2014), the Table 331.1.3 (Exemption to Mandatory Postweld Heat Treatment), the tabulation for P 1 (all groups), it indicated that "All thicknesses" for "All of type of welds" there is no need to perform PWHT. Except that >25mm they need to perform preheat at 95degC.

So based on above, it now looks all thicknesses are exempted from PWHT, and there is no need to even perform preheat for weld thicknesses <=25mm; and if we just perform preheat the PWHT is now exempted for any thicknesses. Table 330.1.1 -2014 indicated Preheat for <=25mm is 10degC (again it is not clear on this 10degC requirement).

Regards
sajid sakhidas
On 17 Dec 2015 05:17, "Pedro JUNIOR" <pedro.junior@total.com> wrote:
>
> Dear experts,
>
>  
>
> I have just one query regarding the Post Welding Heat Treatment as per ASME B31.3_2014, which determines 19mm for Carbon Steel (P number 1) as the minimum thickness for PWHT.
>
> The code indicates the Table 331.1.1 which actually gives us the Holding Temperature Range and time per  the thickness. Can you please give me the right direction (table) to find this statement?
>
>  
>
>  
>
>  
>
>  
>
>  
>
> --
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> To post to this group, send email to materials-welding@googlegroups.com.
> Visit this group at https://groups.google.com/group/materials-welding.
> To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/F259984E42C1CE448E2E2CE7084C2C57013595D4756D%40AOEPTTA-EG11.main.glb.corp.local.
> For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAD%2BGM5XDJ99oavpUstk5jGO%3DozJ259YfEr2wMOM8r2CqOWaepg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMjXr%3DWt4enDhpix_rfqe9gzJ_RKn%3DctZtnkUBftiaVuA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...