What is the confusion?
It is Category B joint. Refer UW-3 (b).

On Dec 17, 2015 9:34 PM, "Chetan" <patilvicky4@gmail.com> wrote:
Dear sir,

Please resolve this confusion about weld joint category.

What's the weld joint category for nozzlE  LWNRF TO SRNECK joint.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5672c298.8e49620a.5c2a3.453a%40mx.google.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKJec9JWNYoLbwhj9xPkBT5O6fZ3vcurHCJk_x1e73_HhDYKLA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...