Dear Mr. Dominic,

Your concern is very relevant. It is a common doubt among young professionals.
Since  WPS qualification in an expensive effort by means of time and cost,mostly companies will go for same document qualification by submitting their existing PQR and WPS for review and approval if there is no much deviation in Essential and supplementary essential variables
 .
ASME permits it as the responsibility of manufacturer/contractor.

Infact , It is the sole discretion of client engineer  whether approve or go for new PQR.

JIJILAL K M
QA/QC Manager,
Jurong Engineering Limited.
TJEL-KCE project,Thailand. 

K.M. JIJILAL


On 19 November 2015 at 00:43, dominic v.k.dominic <v.k.dominic@gmail.com> wrote:
Dear Expertise,
The contractor submitted other project PQR and approved by some other third party company and client.
My Question: Can used other client approved PQR for this new project and new Client?
In the code (API-1104 and ASME Section -IX) anywhere specified in this matter for Employer can be used other project PQR-If matching According the codes and new client requirements.
If yes, please provide code reference.

Thanks in Advance.
Best Regards,
Dominic.



--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/650131b9-29c8-4683-b02f-cb6265988377%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHmEnHjWAGXhgQYm7Qxp8yxJDZCpPAgtP2E2R6_Qv6RvXctz8w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...