Re: [MW:23971] Re: Other Project PQR Can be used New project on Different Clients?

approval/certification only by manufacture not by client. Client  can witness/review, this is as per ASME SEC 9

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY

On Sat, Dec 12, 2015 at 11:29 PM, Shakeel Ahamad <shakeel1378@gmail.com> wrote:
Dear Member,
You can use other project's PQR but on the WPS reflect the name of new owner. For details pls.see the ASME Sec-Ix, QW-201.


Regards,
Shakeel

On Thu, Nov 19, 2015 at 6:29 PM, Sundar Kumar <sunkumarshine@gmail.com> wrote:
Please refer QW-201 Manufacturer's or Contractor's Responsibility (ASME IX - 2011) .It solves your query.

Thanks,
Sundar 

On Thursday, November 19, 2015 at 6:50:01 AM UTC+3, dominic v.k.dominic wrote:
Dear Expertise,
The contractor submitted other project PQR and approved by some other third party company and client.
My Question: Can used other client approved PQR for this new project and new Client?
In the code (API-1104 and ASME Section -IX) anywhere specified in this matter for Employer can be used other project PQR-If matching According the codes and new client requirements.
If yes, please provide code reference.

Thanks in Advance.
Best Regards,
Dominic.



--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9129bd1f-1407-46f3-9799-5f1c37e5fc94%40googlegroups.com.

For more options, visit https://groups.google.com/d/optout.



--

Shakeel Ahamad

 Dy. Manager - Quality

TATA PROJECTS LTD.
Site Office,
RWIS, Visa Power Ltd. Raigarh

Mob.No. 7898361592

Corporate Office
Mithona Tower - 1 Opp. Wesley Co-Ed Jr. College,
Prenderghast Road,Secunderabad - 500003 India.
Email:- shakeelahamad@tataprojects.com
Website:- www.tataprojects.com

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHO2htKFN9zHFCd6bOf7-eSWB3iriCJuHbcVeuPOsy3cnZ-G2A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMC4v1-7586BC5dx6em7Dedm19D6DG_YZ1pmgfo9xqtSw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...