Re: [MW:23956] PQR position conflicts

Position is not an essential variable for PQR

Sent from my BlackBerry 10 smartphone.
From: Narender Reddy
Sent: Τρίτη, 8 Δεκεμβρίου 2015 - 05:28
To: Materials & Welding
Reply To: materials-welding@googlegroups.com
Subject: [MW:23950] PQR position conflicts

Dear experts

As per sec IX

I have an PQR which qualified on 3G(Plate) so


Q.1) Can i use that pqr for to weld 3Nps pipe 6g positions welding.

or is there any conflict between plate and pipe qualification.If there experts can explain why?

Bets regards
reddy.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/eefd149c-2943-4be7-901c-68dc59be172c%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...