RE: [MW:23946] Preheat requirement for EN10225 material

You have to calculate the amount of preheat to the rules in EN 1011-2 as referenced by Georgios Dilintas, knowing the carbon equivalent of the steel, the combined thickness of the steel and the welding heat input. i.e. there is no a single figure answer. Also note that structural steels containing boron are in the market, which increases the hardenability of the steel and the rules of EN 1011-2 are not valid (are not conservative enough) for such steels.

 

Alan Denney

AKD Materials Consulting Ltd

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of george.dilintas@gr.bureauveritas.com
Sent: 04 December 2015 09:05
To: materials-welding@googlegroups.com
Subject: Re: [MW:23945] Preheat requirement for EN10225 material

 

You may find an answer in EN 1011-2, since you are dealing with EN materials

best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04


vijay ---04/12/2015 06:46:32---Gents, Please advise for the minimum preheat recommended for EN 10225 S355G7+M &

From: vijay <vijayakumarme@gmail.com>
To: materials-welding@googlegroups.com
Date: 04/12/2015 06:46
Subject: [MW:23944] Preheat requirement for EN10225 material
Sent by: materials-welding@googlegroups.com





Gents,

Please advise for the minimum preheat recommended for EN 10225 S355G7+M & S355G8 + M Z35 steel grade materials for weld procedure qualification with SMAW process.

Regards,
Vijay

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJ3svCD31EGBwyJy5QR%2BUt2iWLUn90k6ktoYXq_XhGN3ASfpMg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/OF7162FE28.FFA72E77-ONC2257F11.0031CB35-C2257F11.0031DBBE%40LocalDomain.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...