As per API 1104, in addition to tensile strength ( If breaks in weld with strength greater than base metal), u have to check the requirement of soundness of weld. say gas pocket should not be greater than 1.6mm, slag inclusion less than .8, in depth, and not more than 3mm or one half the nominal wall thickness in length. atleast 13mm separation in between slag, if above requirments  are met, then it is acceptable

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY

On Mon, Nov 30, 2015 at 8:01 PM, Vishwas Keskar Welding Manager Pune India <vvkeskar123@gmail.com> wrote:
if the breaking  tensile strength is more than the base metal, then no problem
In PQR , write that "Fracture in Weld "
that's all

On Sunday, November 8, 2015 at 9:43:31 AM UTC+5:30, ahmed boh wrote:
Hi,
I am working in pipeline project API1104.
I heve one speciemen breaks on the weld in tension test for mechanized welding operator with filler metal and the tension strength was greater the SMTS.

 pls advise what we should do in this case?
ahmed

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8341587f-4c0f-457f-8cdf-0b2e90d3861e%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOUxvhjsV2r4kbZ12vbnhVc5knCpbsEni4jdZxj%2BR0SYQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...