Thursday, December 31, 2015

[MW:24018] Re: DIFFERENCE BETWEEN EN-287 OR EN-9606.

Hi,

We need to follow BS EN 9606-1 which supersedes BS EN 287-1.

In BS EN 9606-1, Clause 9.3 has been introduced regarding revalidation of a welder's qualification.

Regards,
Deepak Das.


On Thursday, 31 December 2015 04:41:31 UTC+2, dusroni wrote:
Dear sir,

As per EN Stander we need to do WQT.

kINDLY SUGGEST  WHICH STANDERS TO BE FOLLOW ON THESE TWO-EN-287 OR EN-9606.
kINDLY LET US KNOW THE DIFFERENCE BETWEEN THESE TWO


--
uday

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/78ef7196-1e04-4b9c-9e0c-29a83ddcfdd8%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...