In my opinion compatible would be ERNiCrMo-4  (UNS N10276) 

On Wednesday, December 23, 2015 at 7:37:18 AM UTC+4, rbapat wrote:
Dear Experts
Can a nozzle made of AMS 5390 material be welded to C-276 pipe?
What process and what consumable and any precaution s Are these compatible
Kindly advise
Happy New Year
Ramesh

Sent from my iPhone

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/84a47322-b494-4862-99a1-cddc54bf4332%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...