ASTM HOLE TYPE 15 , WIRE TYPE 1B 11 

On Monday, August 16, 2010 at 11:29:05 AM UTC+4, subrata das wrote:

Dear All

What type of Pentameter should i use during Radiography Test of a butt weld joint of 50 mm diameter & 12 mm thickness and joint between A182 F91(WN Flange) to SB622 UNS N10276(Pipe).

 

Regards

Subrata Das

 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/cf2c6fde-7f9d-4381-a9b9-ec3645dcf556%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS