[MW:23982] RE: 23977] Reg: post welding heattreatment

Rate of cooling and rate of heating shall be as per sec same sec 1. 

Below 300 deg c, air cooling can also be done. 

Regards,
Ram

From: Gopi Nath
Sent: ‎17-‎12-‎2015 12:03 PM
To: materials-welding@googlegroups.com
Subject: [MW:23977] Reg: post welding heattreatment

Sir,
I want to know which standard insist furnace cooling for PWHT
for P1 material

With regards

Gopi

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJK4g1czX52p%2B6eFThNPejV7Wpfm2Z1uYOLtT1egDCpm6mngZw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...