[MW:23964] How to convert groove weld to fillet?

Hi 

In a project the type of weld in the drawings in connection between flange to beam was groove but the welder made a mistake and they executed it as fillet. is there any way that we can convert these two welds to each other ? for example to increase the passes or something like this?


Best regards,

mehdi hoseini

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4357f6ef-12aa-4700-b10a-fbc0f4299abf%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...