[MW:23962] RE: 23961] Tensile specimen size

Please look through Sec-II, Part -A, SA 370 or ASTM- A-370. All necessary details are provided in this standard
 

 

Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Engineering Specialist
Ontario,Canada.
ca.LinkedIn.com/pub/pradip-goswami/5/985/299

pgoswami@quickclic.net

pradip.goswami@gmail.com

All provided answer are personal opinions or personal judgments only. It's not connected with any employers by any means. 

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of sajid ahmad
Sent: Tuesday, December 08, 2015 11:11 AM
To: materials-welding@googlegroups.com
Subject: [MW:23961] Tensile specimen size

Dear experts
I have raw material which details are given bellow.
 Material :                SA 516 Grade 70 N
Thickness of Plate: 50 mm
 I observed during inspection that there is missing of plate mark No.So we are conducting Tensile test in order to co-relate with ASME Sec II.
what will be the specimen size?

Regards

M.S.Ahmad 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAKkJLfgTkvdo37zehERpkPi_kSQeffMmaYgHGS%2BwB91UeZ2gw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...