Saturday, December 14, 2013

Re: [MW:19590] A890 duplex steel casting crack repair.

Hi, 
If possible send pictures of the crack.
How did you find this crack and when?

What is the exact material grade ?

Regards
Praveen

Sent from my iPhone

On 14 டிச., 2013, at 8:20 AM, Abhimanyu Rathore <nice.banna@gmail.com> wrote:

Dear sir,

Can any one provide WPS for crack repair in A890 duplex steel casting.

IS Filler ER 2593 is OK for doing welding.

Thanks in advance.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...