What's the specification/grade of DSS casting to be repaired. You need to specify that. The filler/ electrode used should match the chemical composition of the grade to be repaired.
 
It's advisable to perform  "Soln Anneal" following repair, as per A-890.
 
Appreciate your response.
 
Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Specialist
Ontario, Canada
 
 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Abhimanyu Rathore
Sent: Friday, December 13, 2013 11:21 PM
To: materials-welding@googlegroups.com
Subject: [MW:19588] A890 duplex steel casting crack repair.

Dear sir,

Can any one provide WPS for crack repair in A890 duplex steel casting.

IS Filler ER 2593 is OK for doing welding.

Thanks in advance.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35763] Hardness range for CS+ Alloy0625 clad welding

Dear experts. I am currently in the process of qualifying a PQR for API 5L X65 + A350 LF6. Both material consists of a base metal with alloy...