Sunday, December 1, 2013

Re: [MW:19417] under ground pipeline leak testing method during hydro test

underground pipelines have been hydro tested for a time of duration 1 hrs but line is 1.5 km.this pipeline are tested by without using the pressure and temperature recorder and my question 
why do we want to use this pressure and temperature recorder?
can you give me any detail for this one and send some sample copy format & procedure
  


Regards
HAFEEZ KHAN.G 
 


On Fri, Jan 6, 2012 at 9:35 AM, narasimha murthy <jnm71269@gmail.com> wrote:
Underground lines shall be hydro tested for a time duration of min 24 hrs by using pressure and temperature recorders so that any drop in pressure if noted can be evaluated if its due to temperature variation or due to leakage, this should be a procedure accepted with agreement of the client.

Regards


On Thu, Jan 5, 2012 at 2:49 PM, mohd.qce <mohd52100@gmail.com> wrote:
Dear experts,

Can any one give good and efficient method of underground(buried) pipe
line leak testing method during hydrotest?

Pipe:        API 5L Gr 52 MS PSL-2.
Length :    Two section 50km+50km (2500 joints approx each section).
Test pressure : 73.25 bar.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35006] Difference of 2% of Chromium Content on the Actual PMI VS Sec IIA

Sirs, Do we have supporting verses in ASME? Thanks On Thursday, May 16, 2024 at 5:58:42 PM UTC+8 Mohamed Ali wrote: Kindly get client specif...