Dear pramodh,
ASTM 283 Gr D is equivalent further as per BS4360 its 43B, and as per DIN 17100 its St 44-2
regards,
mohd
On Saturday, July 23, 2011 1:16:35 PM UTC+1, PRAMODH NAIR wrote:
Experts,Could you please give me the equivalent ASTM material for EN S275JR with reference code document.RegardsPramodh
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
Comments