new edition (44th edition) of API 5L/ISO 3183 has these grades, P number is same in ASME (2013 edition) for both these grades
On Sunday, 15 December 2013 10:37:40 UTC+5:30, PRADEEP KUMAR NAIR wrote:
-- On Sunday, 15 December 2013 10:37:40 UTC+5:30, PRADEEP KUMAR NAIR wrote:
WHAT IS BNS IN API 5L. IF X52 MATERIAL QUALIFIED WPS WILL QUALIFY BNS?Can anyone explain?Thanks
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
No comments:
Post a Comment