If both material is of P1
If you qualify PQR of P1 to P1 on 38mm thk plate you are satisfying all condition given in QW 202.4 a and b(2) and with this PQR you can weld between 5mm -200mm thinner component to any thicker component of P1(In your case) of any weld configuration
Regards
Hegde P.B.
----- Forwarded Message -----
From: S.Mohammed <mohd52100@gmail.com>
To: materials-welding@googlegroups.com
Cc: Hardik Pandya <hardik_real@yahoo.co.in>
Sent: Friday, 13 December 2013 1:03 PM
Subject: [MW:19581] Re: Dissimilar Base Metal thikness QW-202.4
From: S.Mohammed <mohd52100@gmail.com>
To: materials-welding@googlegroups.com
Cc: Hardik Pandya <hardik_real@yahoo.co.in>
Sent: Friday, 13 December 2013 1:03 PM
Subject: [MW:19581] Re: Dissimilar Base Metal thikness QW-202.4
Dear sir,
Thanks for reply,
Pl find attachment for Joint Reference,Materials-P1-P1 available WPS qualified up to 20mm
Fig-1 : Considering 202.4 dissimilar joint requirement, base metal qualification up to 65mm need for welding YES/NO
Fig-2 : Considering 202.4 dissimilar joint requirement, base metal qualification up to 65mm need for welding YES/NO
Fig-3 : Considering 202.4 dissimilar joint requirement, base metal qualification up to 65mm need for welding YES/NO
Fig-4 : Considering 202.4 dissimilar joint requirement, base metal qualification up to 65mm need for welding YES/NO
regards,
mohd.
Dear Sir,I have to weld SA 516 Gr.70 (37mm Thk) Tube sheet to SA 516 Gr.70 (10 mm Thk) Shell as per below given weld details.I have Qualified WPS of P1 to P1 material for 20 mm max. Base metal Thikness.Now as per QW-202.4 Thicker member Thickness shall be within the range permitted by QW-451. My thicker member thickness is 37 mm.Kindly pls explain me to can I use WPS yes or No with explanation.RegardsHemant H sutharAsst. Manager QA/QCChemithon Engineers Pvt Ltd.Khanvel-Kheradi Road. Silvassa, UT of DNHWebsite: www.chemithon.co.inOffice Contact: 0260 2677889 / 2677036 , 37 Cell : 9712973092
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
No comments:
Post a Comment