Any subsequent pass after previous pass in tig process could be considered as omalising pass and generally considered in repair welding. Edge overlap is app. 1 to 1-5 mm to avoid umdercuts at the edge and avoid premature failures during uts. bend tests. Sridhar

----------
Sent from my Nokia

------Original message------
From: c.vijay kumar <vijay_online2003@yahoo.co.in>
To: <materials-welding@googlegroups.com>
Date: Friday, September 21, 2012 9:26:25 AM GMT+0800
Subject: [MW:15352] Normalise weld pass

Dear Experts,
 
Can you kindly clarify if the last weld pass is the normalise pass, then how much distance it should be from the edge of the groove. Is there any standard to give the distance in details.
why such a distance need to be maintained.
 
Regards,
Vijay

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...