Hai, usually we do mpi by using permanent magnet in pipes and plates after preparing bevel. This we follows in PDO projects. FYKI. R Vairamuthu, Oman.
Date: Mon, 17 Sep 2012 17:05:56 +0300
Subject: [MW:15332] MPT test method to check the Lamination on the Bevel Edge.
From: biplab.mech@googlemail.com
To: materials-welding@googlegroups.com
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Date: Mon, 17 Sep 2012 17:05:56 +0300
Subject: [MW:15332] MPT test method to check the Lamination on the Bevel Edge.
From: biplab.mech@googlemail.com
To: materials-welding@googlegroups.com
Dear Exparts,
I have a doubt regarding MPT method.
I am going to check the lamination of plates from the bevel edges.
What MPT current mode should we use.
Is it AC or HWDC?
Please share your knowledge and code references.
--
Thanks & Regards
Biplab Pal
Welding Inspector
Biplab Pal
Welding Inspector
E-mail: biplab.mech@gmail.com
Information in this email and any attachments is confidential and intended solely for the use of the individual(s) to whom it is addressed or otherwise directed. Please note that any views or opinions presented in this email are solely those of the author and do not necessarily represent those of the Company. Finally, the recipient should check this email and any attachments for the presence of viruses. Myself accepts no liability for any damage caused by any virus transmitted by this email.
Information in this email and any attachments is confidential and intended solely for the use of the individual(s) to whom it is addressed or otherwise directed. Please note that any views or opinions presented in this email are solely those of the author and do not necessarily represent those of the Company. Finally, the recipient should check this email and any attachments for the presence of viruses. Myself accepts no liability for any damage caused by any virus transmitted by this email.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments