As per knowledge no need to follow the ASME B31.3 IN this case, check and confirm the fit-up in line if fabricated in shop or in field.
Second monitor the joint weld after and during the welding process of two pipes or spools .

Third one , check the straightness of pipe before welding.(solution make straight)

fourth one , check structure alignment is correct or not.(if concrete beam advised to make level )

finally try to put seam to maintain the level .

But After reading your question i am on conclusion that check support weld and welding process .


Thank you.

On Sat, Sep 22, 2012 at 5:34 PM, Biplab Pal <biplab.mech@googlemail.com> wrote:
Dear Experts,
 
We are going to erect the pipe in the pipe rack. The construction is erecting pipe, doing fit-up, and welding. But pipe line in the rack is not straight. they are going the way like snake. Our consturction code is ASME B31.3 process piping. I wanted to know what is the acceptance criteria for the straightness if the line pipe.
Please provide the reference.

--
Thanks & Regards
Biplab Pal
Welding Inspector
E-mail:   biplab.mech@gmail.com
 
Information in this email and any attachments is confidential and intended solely for the use of the individual(s) to whom it is addressed or otherwise directed. Please note that any views or opinions presented in this email are solely those of the author and do not necessarily represent those of the Company. Finally, the recipient should check this email and any attachments for the presence of viruses. Myself accepts no liability for any damage caused by any virus transmitted by this email.
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 



--




With kinds Regards

*********************

PRAVEZ ALAM

MATERIAL/PIPING INSPECTOR

SK E &C

Ruwais Refinery Expansion Project, 

P O Box : 11780, Ruwais,  Abudhabi.

United Arab Emirates.

Mob-+971509867435

E-mail-skec.cv4087@partner.sk.com

            alampravez@gmail.com


"When I am working on a problem I never think about beauty. I only think about how to solve the problem. But when I have finished, if the solution is not beautiful, I know it is wrong."



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...