Dear Sir,
Hi Friends please help me to clear the doubt
I have PQR qualification for 8mm thickness Fillet welding by using E6013 electrode. as per IS 7307 - Part I (1974).
Base material IS 2062 Grade B
Is it necessary to qualify 8mm thick by using E7018 electrode?
4. Changes affecting approval
4.1 A welding procedure test shall be required when any of the following changes are made to an approved welding procedure:
4.1.f ) Any change in type of electrode, filler material, flux or shielding gas.
As per IS 7310 Part I (1974)
5. Extent of approval
5.1 General - The extent of approval for a welding procedure. When a change in the welding procedure according to $ of IS 7307 (part I) - 1974 require a new welding procedure test, this shall entail re-approval of the welder except in the following cases :
c) A change from a basic to a rutile covered electrode.
Please help for a clear answer.
Thanking you for you valuable time you are going to give me in this case.
Dear Sir,
Thanking You.
With Warm Regards,
Muthu barathi P,
Mobile No. 9099006785
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Hi Friends please help me to clear the doubt
I have PQR qualification for 8mm thickness Fillet welding by using E6013 electrode. as per IS 7307 - Part I (1974).
Base material IS 2062 Grade B
Is it necessary to qualify 8mm thick by using E7018 electrode?
4. Changes affecting approval
4.1 A welding procedure test shall be required when any of the following changes are made to an approved welding procedure:
4.1.f ) Any change in type of electrode, filler material, flux or shielding gas.
As per IS 7310 Part I (1974)
5. Extent of approval
5.1 General - The extent of approval for a welding procedure. When a change in the welding procedure according to $ of IS 7307 (part I) - 1974 require a new welding procedure test, this shall entail re-approval of the welder except in the following cases :
c) A change from a basic to a rutile covered electrode.
Please help for a clear answer.
Thanking you for you valuable time you are going to give me in this case.
Dear Sir,
Thanking You.
With Warm Regards,
Muthu barathi P,
Mobile No. 9099006785
| Follow Rediff Deal ho jaye! to get exciting offers in your city everyday. |
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.