Tuesday, September 25, 2012

[MW:15387] Socket weld gap requirement

Dear experts,

Thanks for every comments and suggestions.  Our client point of view, pipe shall be expanded during operation.

Material: A312 TP316L
Size:1 ½",1" Sch40
Design temp.:96 C
Operating temp.:68 C
 
Thanks & Regards,
Naresh


From: Naresh Kumar <snareshkumar30@yahoo.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Saturday, September 22, 2012 8:21 PM
Subject: Socket weld gap requirement



Dear experts,

As per ASME 3.1.& 31.3 socket weld gap requirement is 1/16" before welding. Whether it is required for after welding, if its require kindly provide the code details.In our project we're done RT for socket welds. But after welding did not find the 1/16" gap, its less than 0.5mm. Our client decision is to cut and reweld the all joints.
 
 
Thanks & Regards,
Naresh




No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...