Thursday, September 27, 2012

Re: [MW:15408] Repair after PWHT - B 31.1

For repair carried out after pwht than pwht is mandatory after repair if service requirement.
If as per code than exemption clause shall be applicable based on depth of repair.

On Sep 19, 2012 3:07 PM, "Muhammed Ibrahim PK" <ibratech@gmail.com> wrote:
Double PWHT will reduce tensile strength.

Thanks & Regards
Muhammed Ibrahim PK



On 18 September 2012 00:53, sabi sabi <sabi2kg@gmail.com> wrote:
Dear gents,
 
Case-1: Normal practice
1.welding (with/without pre heat & post heat)
2.RT
3.Clear repair + RT
3.PWHT
4.RT
 
Case-2: Some agents are doing (with confidence of worker & Did not get a time fot RT)
1.welding (with/without pre heat & post heat)
2.PWHT
3.RT
4.Clear repair (with/without RT)
5.PWHT
6.RT
 
Solution of case-2: There is no problem for twice PWHT. It will not affect any meterial properties.
 
That is the reason, we are taking hardness test to meet requirement. Only time will take more.
 
Regards,
sabi
 
 
On Mon, Sep 17, 2012 at 10:01 AM, Muhammed Ibrahim PK <ibratech@gmail.com> wrote:
PWHT shall be done after repair. To avoid this issue better to perform RT before PWHT also.

Thanks & Regards
Muhammed Ibrahim PK



On 10 September 2012 09:10, sevak hiren <hirensevak80@gmail.com> wrote:
Dear Experts,

Piping Code : ASME B 31.1, Power Plant Piping, (P No.5A,11,12,15, 91 etc pipes) & ASME Sectin I

Contractor is doing piping fabrication stages in following manner,

Preheating & Welding of Piping joints then Post heating, then PWHT & then finally RT.

Contractor is arguing, RT is taken after PWHT  to reveal the defects causing due to delayed cracking.

My question

If RT repair is done for particular joint after PWHT then is it compulsory to perform PWHT again for particular joint ? if yes then please mention the clause of code.

Thanks & Regards

Hiren Sevak






--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...