Dear Sasi,
You can ask the lab to do hardness testing on weld metal, HAZ and parent
Metal, the location shall be weld top, weld middle and weld bottom same with
HAZ.
With kind regards,
Vinod Kataria
General Manager
Bliss Anand Private Limited,
92B/93B Sector 5
IMT Manesar,Gurgaon,
National Capital Region Delhi.
India .
Phone : +91-124-4366000 (9 Lines)
Mobile Phone : +91-9560199004
Fax : +91-124-2290884
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Sasi
Sent: Friday, September 28, 2012 3:22 PM
To: materials-welding@googlegroups.com
Subject: [MW:15417] HARDNESS and Macro location
Dear sirs
I already done Procedure Qualification Test as per ASME Sec IX and sent it
for mechanical and Destructive testing. The LAB people they are saying to
detemine the location of Hardness testing and Macro testing. How I can reply
to them. Please advise me . Quick reply , it will be very useful to me.
Thanks and Regards
Sasikumar.R
This e-mail and any files transmitted with it are for the sole use of the
intended recipient(s) and may contain confidential and privileged
information. If you are not the intended recipient of this communication, we
request you to notify the sender immediately by return email and destroy all
copies and the original message. Any unauthorized review, use, disclosure,
dissemination, forwarding, printing or copying of this email is strictly
prohibited.
The recipient acknowledges that Punj Lloyd Limited or its subsidiaries and
associated companies (collectively "Punj Lloyd Group") are unable to
exercise control or ensure or guarantee the integrity of/over the contents
of the information contained in e-mail transmissions and further
acknowledges that any view, opinion or advice expressed in this message are
those of the individual sender and no binding nature of the message shall be
implied or assumed unless the sender does so expressly with due authority of
Punj Lloyd Group.
Although we have taken all reasonable precautions to ensure that this
communication is free from viruses. We do not assume responsibility for any
loss or damage arising from the use of this email.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=
<http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk
=anet_ug_hm> &gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
[MW:35633] IP Joint
Hello experts, I would like to know what is IP joints in piping(31.3)? Regards Saurabh -- https://materials-welding.blogspot.com/...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment