Re: [MW:15400] ALIGNMENT OF LINE

This is purely under juriscation of Client specifications.
It is usually the asthetics that influences the tolerences but in some cases it is need of application too like in one of my jobs I had to allign within + 0.5 which is very rear in normal applications.
 
Ammar

On Wed, Sep 26, 2012 at 12:36 AM, Dr-alaa Zg <dralaazg@yahoo.com> wrote:
Dear Sampath

Tolerances of pipe lines are generally given in the contract documents or in  PFI standards ES02 and ES03. 

Best of regards

Dr. Eng. Alaa A. Atiyah
Technical Manager
Delta Integra Group 

--- On Tue, 9/25/12, Sampath Kumar <skthatham@gmail.com> wrote:

From: Sampath Kumar <skthatham@gmail.com>
Subject: [MW:15388] ALIGNMENT OF LINE
To: materials-welding@googlegroups.com
Date: Tuesday, September 25, 2012, 2:50 AM


Hello Everybody,
 
can anybody give some facts related to the tolerance/allowance limit with regards to "ALIGNMENT OF LINE",both Horizontal & vertical of any given size with some code and standarad referrence.
 
Thanks & Regards
 
sampath
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...