Friday, September 21, 2012

[MW:15352] Normalise weld pass

Dear Experts,
 
Can you kindly clarify if the last weld pass is the normalise pass, then how much distance it should be from the edge of the groove. Is there any standard to give the distance in details.
why such a distance need to be maintained.
 
Regards,
Vijay

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 