Re: [MW:15339] IQI SELECTION

Dear brother,
 
Any RT job, IQI selection is for sigle wall thick.
 
But you have think about which side to be use. If it is film side, to use with letter "F".
 
Expore time only will change according the technique.
 
Thanks,
Sabi

On Sun, Sep 16, 2012 at 9:40 PM, manoj nadar <manojnadar007@gmail.com> wrote:
dear experts,
I got a prob in selecting IQI for DWSI pipe.
for eg, I select a pipe of 9mm single wall thickness and reinforcement
is 3mm i read that i must use single wall thickness to select IQI but
now I select a weld joint of 21mm thickness what IQI will u choose for
that.
as both job are given same time how could we expect to see different
wires am confused pls help

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...