Re: [MW:15413] Welding consumable for welding of CS to Cast Iron


MR RANENDRA ,



let me have the material specification details so that one can have the full
details
ex: like is 2062 gr a material to is 2062 gr a
is 2062 gr b to gr b

even the welding consumable will be specified on the type of the job

usually for low strength we use E6013. if it need to with stand more strength we
will be going for low hydrogen electrode like E7018 .

. if we use is 2062 gr a to is 2062 gr a material and if it need withstand good
strength then we need to go for E9018. as u may be aware that pre heating of
electrode and all .

i think after going through this u may be having a good idea if u need more u can
mail me


Regards,
srikkanth
On Wed, 26 Sep 2012 16:48:09 +0530 wrote
>Dear Experts,
Please guide which kind of consumable can be used for welding of CS with Cast
Iron.
 
Ranendra Chakraborty



--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-
welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-
welding.blogspot.com/
>
http://www.linkedin.com/groups/MaterialsWelding-122787?
home=&gid=122787&trk=anet_ug_hm
>

>
The views expressed/exchnaged in this group are members personel views and meant
for educational purposes only, Users must take their own decisions w.r.t.
applicable code/standard/contract documents.
>

>

>


Follow Rediff Deal ho jaye! to get exciting offers in your city everyday.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...