no it it not required after welding, many times gap closes to zero due
to shrinkage during welding. if your client requires the gap after
welding (I don't see any reason for this) probably you need fit up
with more gap.
On Sep 22, 7:49 pm, Naresh Kumar <snareshkuma...@yahoo.com> wrote:
> Dear experts,
>
> As per ASME 3.1.& 31.3 socket weld gap requirement is
> 1/16" before welding. Whether it is required for after welding, if its require
> kindly provide the code details.In our project we're done RT for socket welds. But
> after welding did not find the 1/16" gap,
> its less than 0.5mm. Our client decision is to cut and reweld the all joints.
>
>
> Thanks & Regards,
> Naresh
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
[MW:35668] Selection of Filler/Electrode.
Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-