Re: [MW:12704] ASTM A106 Grade B

Dear Mr. Vivek,

According to para. 4.1 of ASTM A 106, it seems that it should be fully Killed but I think Experts and Manufacturer can help.


4. Process
4.1 The steel shall be killed steel, with the primary melting
process being open-hearth, basic-oxygen, or electric-furnace,
possibly combined with separate degassing or refining. If
secondary melting, using electroslag remelting or vacuum-arc
remelting is subsequently employed, the heat shall be defined
as all of the ingots remelted from a single primary heat.


Kind Regards,
Zarei


On Tue, Oct 18, 2011 at 7:45 AM, Vivek Joshi <hifromvivek@gmail.com> wrote:
Hello everybody,
Can somebody tell me please whether ASTM A106 Grade B is fully killed
steel by ASTM specification itself. If not then is it also avalable in
the form of Semi-Killed steel.
Vivek

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...