Dear Vivek
 
Code says only killed steel , i.e manufacture will furnish the same in semi killed also. If you required Fully killed material then you have to carry out O2 analysis.
 
Regards
Hitesh

On Tue, Oct 18, 2011 at 9:45 AM, Vivek Joshi <hifromvivek@gmail.com> wrote:
Hello everybody,
Can somebody tell me please whether ASTM A106 Grade B is fully killed
steel by ASTM specification itself. If not then is it also avalable in
the form of Semi-Killed steel.
Vivek

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...