Re: [MW:12795] PIPE TO WLDOLET JOINT THICKNES

Based on the type of fit-up if Stub-in Run pipe thicknes or if
Stub-on Branch pipe thickness.

Liyakath alik A

On 10/26/11, Mohamed Khaleel <smohdkhaleel@gmail.com> wrote:
> Run pipe to banch connection through weldolet fitting used. i need to
> know what is the joint thicknes considered for selection of WPS. For
> Ex. thickness at 6" run pipe to 2" weldolet branch.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...